Coating Weight Selection for Industrial Atmospheres with High SO₂ (ISO 9223 C3–C5)

Nov 12, 2026

Leave a message

info-640-300

Most specifications that reach us name a corrosivity category and a coating mass, then treat the two as separate decisions. On a site with sulfur dioxide they are the same decision. The category says how much metal the atmosphere removes each year; the coating mass says how much metal there is to remove. Both numbers have to come from the same site data.

 

In practice the coil is normally fixed first, from habit or from a previous job, and the category is attached afterwards to justify it. That order explains most of the under-specified industrial orders we are asked to correct.

 

Mechanism: what the sulfate film does

 

SO₂ has to deposit before it does anything. On a wet surface it oxidises to sulfate and the film turns acidic; exposed steel in polluted industrial districts commonly sits at pH 3 to 4. That film is the exposure that counts, and on a sheltered face it stays put long after the rain has passed.

 

Zinc forms a mixed hydroxide-carbonate-sulfate product. While sulfate is a minor constituent the product holds back further attack reasonably well. As deposition rises it becomes sulfate-dominated and more soluble, rain removes it, and fresh zinc is exposed. The surface renews itself and the mass keeps falling. The ISO 9223 first-year rates for zinc put loss at 0.7 to 2.1 µm in C3, 2.1 to 4.2 µm in C4 and 4.2 to 8.4 µm in C5.

 

The zinc vs galvalume SO2 comparison usually gets answered with salt-spray hours, and ASTM B117 measures chloride rather than sulfur, so the figure describes a different pollutant. In 55 % Al-Zn the protection sits in the aluminium-rich dendrites: aluminium oxide is stable across the near-neutral range a sulfate film actually reaches, and aluminium sulfate is considerably less soluble than zinc sulfate, so the corrosion product stays where it formed instead of washing off.

 

Category assignment: measured value against description

info-597-336

 

ISO 9223:2012 sets C1 to CX from first-year mass loss on standard coupons. ISO 9225 covers pollutant sampling, ISO 9226 the coupon exposure, ISO 9224 the reference values behind the class limits. ISO 12944-2 uses the same letters for an environment description, which is what a drawing normally carries. Both are legitimate and they do not always agree: a plant a drawing labels an ISO 9223 C4 industrial atmosphere can measure C5 on zinc where the coupons stand under a canopy. When the two diverge, the coupon wins.

 

Where no deposition data exists, ISO 9223 allows an informative estimate from local conditions, which is what many projects have on hand. It is worth having as a starting point. P2 tops out at 80 mg/m²/day and P3 runs to 200; a site can move from one class letter to the next without anything a visitor would notice.

 

Chloride and sulfur also combine badly. A coastal industrial site carrying S1 chloride with P1 sulfur moves zinc faster than either pollutant does on its own, and a plant within a few kilometres of the sea is worth asking for both deposition figures.

 

Mass, converted and worked through

Designations state mass over both faces. Z275 leaves a face with 137.5 g/m², and at 7.14 g/cm³ that is 19.3 µm. The reverse conversion is the one worth remembering: 1 µm of zinc is about 7.14 g/m², so a face losing 3 µm a year loses roughly 21 g/m² a year. Divide 137.5 by 21 and a Z275 face reaches bare steel in about six and a half years. That uses the first-year rate, which is harsh, since ISO 9224 reference values drop as the corrosion product matures; read six years as a floor rather than a forecast. It still explains why a fifteen-year C4 building cannot be bought on coating mass alone where the face is sheltered.

AZ150 leaves a face with 75 g/m², and at an alloy density near 3.7 g/cm³ that is about 20 µm, thicker than Z275 at a lower mass. A good share of the "150 looks thinner than 275" questions we answer begin at that arithmetic. EN 10346 states the nominal mass with a permitted low limit, so a single-spot check on a sound coil can read under the figure printed on the tag.

info-726-726

Coating weight for industrial SO2 environment: the ranges we quote

 

Column two is the measured category rather than the description on the drawing. ASTM A653 G90 and ASTM A792 AZ150 are the closest American equivalents in the first two coating columns.

 

Table 1 Coating mass by SO₂ class, nominal total on both faces to EN 10346

SO₂ class

Measured category

Zinc

Al-Zn

Organic coating

Low

C2–C3

Z120–Z180

AZ100–AZ150

Optional

Moderate

C3–C4

Z180–Z275

AZ150–AZ200

Advised

High

C4–C5

Z275

AZ200

Required

 

Z275 is where we stop on continuously galvanized building coil. Above it price climbs faster than life and the tolerance band widens in grams. On a sheltered C5 face the proposal is AZ200 with a coating system, not Z350 without one.

 

Cut edges and acid condensate

 

A slit or punched edge is bare steel, and only zinc protects it galvanically. In 55 % Al-Zn about 43 % of the coating is zinc, sitting in narrow interdendritic channels that end at the sheared face, so that protection travels a short distance. Trapezoidal decking cut every 600 mm and fixed with self-drilling screws generates a lot of such edges, and on those profiles we specify Z275 even where the surface rate argues for the alloy.

 

Aluminium passivity has a pH floor near 4. In acid dew the alloy gives up the advantage it holds in near-neutral condensate, which puts a heavy SO₂ site with acid condensation into the category where the barrier coating is doing the work.

 

Paint as part of the system

 

An organic coating adds no metallic reserve. It delays the pollutant's arrival and shifts failure to underfilm creep from scratches and sheared edges. Where deposition sits in P2 or P3, the face is sheltered, and the target life runs past fifteen years, we treat painting as part of the system rather than an upgrade. Pretreatment has to match the substrate: an aluminium-bearing surface and a zinc surface take different conversion layers, and a line applying one to both shows it at the cut edges first.

 

EN 10169 governs the organic-coated product. ISO 12944-5 governs the system where the steel is a structure designed to a durability class rather than a cladding sheet.

 

Site data, and what happens without it

info-2500-886

 

Four inputs settle the recommendation: SO₂ deposition in mg/m²/day, or the annual mean concentration in µg/m³ from a station within a few kilometres; whether the surface is rain-washed or sheltered; the service life to be reached; and the cut-edge density the profile creates. A painted finish is normally settled before anyone asks us.

 

Most enquiries arrive without deposition data. We quote the class the drawing names, print the assumption on the order confirmation, and set out in the offer what that coating can and cannot do at that class. It is a weaker basis than measurement, and it is written where the buyer can see it, which is the part that matters.

 

Coils ship with the mill certificate to EN 10204 3.1. Where a project is signed against P2 or P3, we ask for a gravimetric check to ISO 1460 on a sample from each coil before dispatch.

 

Deposition figures, drawings and cut-edge details can go to our sales desk; the reply will carry the mass, the substrate, and the assumption we used.

 